Solid-state lithium batteries

How do interfacial voids evolve under pressure?

At a lithium-metal interface, vacancy diffusion can enlarge a void while creep under pressure can close it. The simulations compare how current, pressure and initial shape affect this competition.

Computed vacancy concentration around three lithium-interface voids
Vacancy concentration · 298 K · 0.5 MPa · 0.1 mA/cm² · 0.01 s

Which processes drive cavity-wall changes?

At each step, the model updates the pore wall using vacancy transport, elastic deformation and creep.

Schematic loading and transport directions around an interfacial void
Lithium metal is on the left, electrolyte on the right, with an interfacial void. Arrows indicate loading and transport; geometry is schematic.

Lithium stripping generates vacancies on the contacting interface. Local current concentration changes the supply near a void.

How does pressure change cavity growth?

At 298 K and 0.1 mA/cm², these two initially semicircular-void cases show how pressure changes the balance between vacancy supply and creep.

298 K 0.1 mA/cm²Initial radius ≈ 1 μm

1 MPa

Recorded to 3.9 s
Void-wall shape and surface vacancy flux at 1 MPa, t = 3.9 s

Saved evolution

Growth continues in this case.

4 MPa

Recorded to 0.5 s
Void-wall shape and surface vacancy flux at 4 MPa, t = 0.5 s

Saved evolution

Creep-induced contraction suppresses growth in this case.

The two recordings use their own physical times and flux scales.

How do initial shape and neighboring voids matter?

Local stress concentration changes the early creep response. When voids coexist, their fields interact and a void can evolve differently from an isolated one.

Irregular void evolution at 298 K, 1 MPa and 0.1 mA/cm², t = 4.98 s; surface vacancy flux
Irregular initial shape · 1 MPa · 4.98 s. Gray: initial wall.
Red isolated-void outline and blue outline of the large void in a three-void configuration at 9.88 s
Red: isolated void. Blue: the large void with neighbors. Recorded case: 0 MPa, 0.1 mA/cm², 9.88 s.
View single- and three-void stress and vacancy fields
Original single-void and three-void von Mises stress and vacancy concentration panels, with independent scales
298 K · 0.5 MPa · 0.1 mA/cm² · 0.01 s. Top: von Mises stress. Bottom: vacancy concentration. Each panel retains its own scale.

What pressure suppresses void growth?

At specified current and temperature, compare critical pressures using the study’s net-void-growth criterion. The curves compare one, two and three voids while keeping total void area and total interfacial contact length constant.

Original critical-pressure versus current-density curves for one, two and three voids at 298 K and 353.15 K
Horizontal: critical pressure / MPa. Vertical: current density / mA·cm⁻². Blue: one void; yellow: two; red: three. Solid: 298 K; dashed: 353.15 K. The 0.6 × single-void curve is an empirical correction in this comparison.

Model and research notes

These two-dimensional stripping calculations use an ideal contacting interface, a rigid-electrolyte approximation and a fitted interfacial-current distribution. The criterion concerns short-time void growth in the modeled conditions; it does not establish a full-cell lifetime or a generally safe operating pressure.

Yibin Jiang & Pengyang Zhao · coupled numerical study