LAwave estimates effective elastic modulus from surface-wave speed and leaves the specimen available for repeat measurements. In printed 316L steel, we compare this modulus with porosity measured by electron microscopy before and after densification.
LAwave apparatus · probe and metal specimen
What can a nondestructive measurement tell us?
Preserve the specimen
The wave causes elastic deformation, so the specimen can be tested again. For thin films, EN 15042-1:2006 describes how laser-induced surface waves can be used to determine elastic constants, density and thickness.
Pores affect effective stiffness. For each group of 316L specimens, we compare LAwave modulus with porosity measured by scanning electron microscopy to see how both change after hot isostatic pressing.
A laser pulse launches a wave along the specimen surface. In the silicon wafer experiment, we recorded four waveforms. The same wave packet arrives later after travelling farther.
Build the dispersion curve from phase differences
At each frequency, the phase difference and the spacing between measurement positions give the phase velocity. Plotting velocity against frequency gives the dispersion curve. Higher frequencies are more sensitive to the near-surface region, while lower frequencies probe deeper.
Estimate modulus and film thickness
For a bulk specimen, wave speed, density and other material properties give an estimate of effective elastic modulus. For a coating, we fit a film–substrate model to the measured dispersion to estimate thickness and modulus. The copper film on silicon in our coating study had a fitted thickness of 40 nm.
How processing changes measured properties
The 316L study pairs modulus with porosity before and after densification. IN718 shows the change in stiffness after heat treatment. The remaining cases compare tensile measurements, build directions and coating thicknesses.
IN718: resolve the effect of heat treatment
Heat treatment raised the mean acoustic Young’s modulus of IN718 from 203.81 to 211.08 GPa.
View measurement data
316L: composition, pores and modulus
After hot isostatic pressing, the acoustic Young’s modulus of the high-silicon group (1.14 wt% Si) rose from 176.39 to 191.90 GPa. SEM porosity fell from 0.89% to 0.49%.
View measurement data
Build direction and elastic response
Measure additively manufactured TC4 and TA15 titanium alloys along the build direction and parallel to the layers, comparing directional differences associated with the printed structure.
Tested materials
TC4 / Ti-6Al-4V TA15 / Ti-6.5Al-1Mo-1V-2Zr
What it supports
Measured evidence for directional property assessment, process comparison and material parameter selection.
Coating thickness and elastic parameters
Our Cu/Si and SiO₂/Si measurements combine dispersion curves with layered-material models to analyze substrate elasticity, coating modulus and thickness.
For coating development and thin-film process comparison.
View measurement data
Analyze film thickness together with coating and substrate elasticity to compare coating systems and preparation states.
Compare elastic response in bulk materials
View measurement data
How to read these measurements
Charts show measured means and the supplied ± ranges for each record. Decimal places and range widths alone do not establish the absolute accuracy of different methods.
LAwave samples effective elasticity over a measurement region; nanoindentation probes local contact response. Pore morphology and statistics come from independent SEM. Structural interpretation uses complementary evidence rather than individual-pore imaging.
Surface-wave sampling depth varies with frequency. Attenuation, surface condition and signal quality affect applicability. The 40 nm and 280 nm values are fitted thicknesses in the corresponding film cases.
Surface-wave analysis with LAWave Insight
Follow four recordings from one silicon wafer in LAWave Insight. Compare wave packet arrival times, then use the phase differences at each frequency to calculate the dispersion curve.
Track the same wave packet across distances
The four silicon-wafer measurements span 0 to 5 mm. The same wave packet arrives later at greater distances.
The workbench plots phase velocity by frequency, marks reliable points and can overlay the instrument’s exported curve. Use the selected band to estimate bulk elasticity or fit coating thickness and modulus with a layered model.
We are developing deep learning models to compare wave packet arrival times, amplitudes and shapes across distances, and to investigate which changes are associated with pores and other microstructural features.
In 316L, we have measured effective elasticity and independently assessed porosity by scanning electron microscopy. These observations provide a way to test the waveform features the models identify.
As-printed high-silicon 316L · scanning electron microscopyFurther work on processing and residual stress
Varying laser power and scan speed would allow comparisons of processing conditions, acoustic response and porosity. Independent stress measurements would also be needed to distinguish the effects of residual stress and microstructure on wave speed.