How defects change material properties

Specimens of the same alloy can yield or fracture differently. Dislocation slip leaves permanent strain, grain boundaries can obstruct slip, and pores shift the load onto the surrounding metal.

Colored dislocation lines on several slip systems in a three-dimensional simulation
Simulated dislocation lines piling up near a subgrain boundary.

Four ways a crystal departs from perfect order

The dimension describes the extent of the disturbance in the lattice. A missing atom occupies one site. A pore has an internal surface enclosing a volume.

0DPoint defectsVacancy schematic
Vacancies and solute atoms

An atom can jump into a vacant neighboring site. Repeated jumps transport matter. A solute that distorts the lattice can also resist dislocation glide.

1DLine defectsEdge dislocation schematic
Dislocations

A dislocation marks the edge of a region that has slipped. As the line moves across a crystal, it leaves a permanent displacement behind.

2DPlanar defectsGrain boundary schematic
Grain boundaries, twin boundaries and stacking faults

Grains meet at different orientations. A dislocation arriving at their boundary may have to change slip system to continue. In a twin the two lattices are mirror-related. A stacking fault interrupts the normal layer sequence.

3DVolume defectsPore in section schematic
Pores and inclusions

A pore removes load-bearing material. An inclusion occupies space but can deform differently from the matrix. Both redistribute stress according to their shape and surroundings.

When slip becomes harder, yield strength rises

At small strains, stretching atomic bonds gives a largely reversible response. Yielding begins when enough slip accumulates to leave a permanent strain. In many polycrystalline metals, refining the grains shortens the unobstructed slip distance and raises the stress needed for yielding.

NN-mGSF connects layer energies to twin growth in copper

NN-mGSF predicts coupled energies from slips on neighboring planes, saving repeated atomistic calculations. For copper, it gives a coherent twin-boundary migration barrier of 137.7 mJ/m², close to the embedded-atom result of 139.1 mJ/m².

Dislocation field dynamics combines the energy gradient with long-range elasticity. In a 30-plane copper simulation, the same twin embryo lengthened under 2.5 GPa shear and also thickened layer by layer at 3.0 GPa.

Explore the layer-energy model
Model input · relative shifts of neighboring layers (schematic)
A red copper twin band within the blue matrix in the simulation
Simulation · watch the twin band grow

From dislocation pile-ups to void nucleation

When a dislocation stalls, others can pile up behind it on the same slip plane. Their stresses add near the head of the pile-up. Our simulations track several groups at a subgrain boundary to examine where local tensile stresses can favor void nucleation.

Explore the dislocation simulation

A pore changes the load path

Under tension, the metal between neighboring voids carries the load. A thinning ligament can rupture and join two voids, one route to ductile fracture. Even at small, reversible strains, pores can reduce the effective stiffness of the whole specimen.

Simulation follows the pore wall

In our single-void calculations, transport along the surface smooths wall undulations. When bulk diffusion dominates under nonuniform stress, the void grows preferentially in one direction and develops tips. The outlines show why porosity alone cannot describe the shape.

Compare the two simulations
Simulated outline of a smoothing pore wall
Surface diffusion dominates
Simulated outline with pointed lobes
Bulk diffusion dominates

Measurement connects pores with stiffness

For printed 316L stainless steel containing 1.14 wt% silicon, we compared the as-printed and hot-isostatically pressed states. Electron microscopy measures porosity and surface waves probe effective Young’s modulus. Together they show how both quantities changed after treatment.

Explore the 316L measurements
Scanning electron micrograph of the as-printed high-silicon 316L specimen
As-printed 316L · electron micrograph
MeasurementAs printedAfter HIP
Porosity0.89%0.49%
Modulus (GPa)176.39191.90

MPTT accelerates the elastic solve around pores

Each change in pore shape and mesh calls for a new elastic solution. MPTT predicts displacement on the current mesh, then PCG refines it to an equilibrium residual tolerance of 10⁻⁵. Across 500 remeshes in the two-pore case, the full run, including diffusion, wall motion and I/O, was 1.96 times faster than FEM.

Compare pore evolution, wall errors and timing